Industrial use cloth
The company mainly produces T/C fabrics, industrial use fabrics, water-jet satin, rayon lining twill, polyester taffeta, polyester trilobal, polyester pongee, case & bag fabric, chiffon etc.. -
TS-PE1238
Breaking Strength(N/5x20cm)in warp/weft:3509.8/2027.8 Enlongation at Break(%)in warp/weft:64.85/53.05 Air Permeability(200 Pa):2774.5 Thickness(mm):0.75 Weight(g/sm):483 finish:Rinse, heatset, ca... -
TS-PE798
Breaking Strength(N/5x20cm)in warp/weft:3239.3/1980 Enlongation at Break(%)in warp/weft:31.6/12.8 Air Permeability(200 Pa):18.4 Thickness(mm):0.75 Weight(g/sm):443 finish:Rinse, heatset, calender... -
TS-PE729
Breaking Strength(N/5x20cm)in warp/weft:3454.8/2025.4 Enlongation at Break(%)in warp/weft:21.3/13.1 Air Permeability(200 Pa):161.9 Thickness(mm):0.65 Weight(g/sm):350 finish:Rinse, heatset, calen... -
TS-PE621
Breaking Strength(N/5x20cm)in warp/weft:2166.7/888.2 Enlongation at Break(%)in warp/weft:28.1/23.5 Air Permeability(200 Pa):12.15 Thickness(mm):0.33 Weight(g/sm):218.89 finish:Rinse, heatset, cal... -
TS-PD4212
Breaking Strength(N/5x20cm)in warp/weft:2217/1244.9 Enlongation at Break(%)in warp/weft:71.9/33.2 Air Permeability(200 Pa):124.8 Thickness(mm):1.35 Weight(g/sm):420 finish:Rinse, heatset, calende... -
TS-PARC2084
Breaking Strength(N/5x20cm)in warp/weft:4707/1355.10 Enlongation at Break(%)in warp/weft:27.15/19.30 Air Permeability(200 Pa):111.67 Thickness(mm):0.57 Weight(g/sm):416 finish:Rinse, heatset, cal... -
TS-PAEC2015
Breaking Strength(N/5x20cm)in warp/weft:4197/3336.9 Enlongation at Break(%)in warp/weft:25.4/20.4 Air Permeability(200 Pa):314.98 Thickness(mm):0.5 Weight(g/sm):381.03 finish:Rinse, heatset, cale... -
TS-PA663826
Breaking Strength(N/5x20cm)in warp/weft:3086.10/2600.10 Enlongation at Break(%)in warp/weft:36.95/32.95 Air Permeability(200 Pa):1117.8 Thickness(mm):0.66 Weight(g/sm):450 finish:Rinse, heatset, ... -
TS-PA83828
Breaking Strength(N/5x20cm)in warp/weft:3387.7/1984.7 Enlongation at Break(%)in warp/weft:26.9/19.55 Air Permeability(200 Pa):2271.5 Thickness(mm):0.81 Weight(g/sm):356.7 finish:Rinse, heatset, c... -
TS-PA63821
Breaking Strength(N/5x20cm)in warp/weft:3684.6/1352.7 Enlongation at Break(%)in warp/weft:34.45/29.05 Air Permeability(200 Pa):908 Thickness(mm):0.57 Weight(g/sm):347.3 finish:Rinse, heatset, cal... -
TS-PA62330
Breaking Strength(N/5x20cm)in warp/weft:4242.5/3357.8 Enlongation at Break(%)in warp/weft:27.8/25.6 Air Permeability(200 Pa):412 Thickness(mm):1.03 Weight(g/sm):607.7 finish:Rinse, heatset, calen... -
TS-PA32378
Breaking Strength(N/5x20cm)in warp/weft:4673.4/2276.8 Enlongation at Break(%)in warp/weft:30.65/18.05 Air Permeability(200 Pa):685.33 Thickness(mm):0.91 Weight(g/sm):500 finish:Rinse, heatset, ca... -
TS-PA4242
Breaking Strength(N/5x20cm)in warp/weft: Enlongation at Break(%)in warp/weft: Air Permeability(200 Pa): Thickness(mm): Weight(g/sm): finish:Rinse, heatset, calenderd -
TS-NOMEX
Breaking Strength(N/5x20cm)in warp/weft: Enlongation at Break(%)in warp/weft: Air Permeability(200 Pa): Thickness(mm): Weight(g/sm): finish:Rinse, heatset, calenderd -
TS-MP922
Breaking Strength(N/5x20cm)in warp/weft:3464.4/2401.3 Enlongation at Break(%)in warp/weft: Air Permeability(200 Pa): Thickness(mm): Weight(g/sm): finish:Rinse,... -
TS-KP96
Breaking Strength(N/5x20cm)in warp/weft:3957.6/1246.8 Enlongation at Break(%)in warp/weft:17.35/11.2 Air Permeability(200 Pa):194.46 Thickness(mm):0.9 Weight(g/sm):4.6 finish:Rinse, heatset, cale... -
TS-ED3927
Breaking Strength(N/5x20cm)in warp/weft:4096.4/3722.9 Enlongation at Break(%)in warp/weft:47.8/21.2 Air Permeability(200 Pa):15 Thickness(mm):1.00 Weight(g/sm):576 finish:Rinse, heatset, calender... -
TS-ED729
Breaking Strength(N/5x20cm)in warp/weft:3536.2/2159.5 Enlongation at Break(%)in warp/weft:28.3/23.45 Air Permeability(200 Pa):50.27 Thickness(mm):0.648 Weight(g/sm):359.6 finish:Rinse, heatset, c... -
TS-DPP59
Breaking Strength(N/5x20cm)in warp/weft:421.3/495.5 Enlongation at Break(%)in warp/weft:27.10/17.35 Air Permeability(200 Pa):3958.2 Thickness(mm):0.1 Weight(g/sm):60 finish:Rinse, heatset, calend... -
TS-COTTON
Breaking Strength(N/5x20cm)in warp/weft: Enlongation at Break(%)in warp/weft: Air Permeability(200 Pa): Thickness(mm): Weight(g/sm): finish:Rinse, heatset, calenderd -
TS-ACLW
Breaking Strength(N/5x20cm)in warp/weft:1000/1300 Enlongation at Break(%)in warp/weft:25/40 Air Permeability(L/sm.s)(200 Pa):1400 Thickness(mm):2.2 Weight(g/sm):500 finish:Rinse, heatset, calende... -
TS-PA6050
Breaking Strength(N/5x20cm)in warp/weft: Enlongation at Break(%)in warp/weft: Air Permeability(200 Pa): Thickness(mm): Weight(g/sm): finish:Rinse, heatset, calenderd